孙庆祖, 黄原定, 杨王玥, 陈国良. Fe3Al金属间化合物的韧化(I)[J]. 工程科学学报, 1991, 13(6): 539-543. DOI: 10.13374/j.issn1001-053x.1991.06.023
引用本文: 孙庆祖, 黄原定, 杨王玥, 陈国良. Fe3Al金属间化合物的韧化(I)[J]. 工程科学学报, 1991, 13(6): 539-543. DOI: 10.13374/j.issn1001-053x.1991.06.023
Sun Qingzu, Huang Yuanding, Yang Wangyue, Chen Guoliang. The Ductility of Fe3Al Intermetallic Compounds (I)[J]. Chinese Journal of Engineering, 1991, 13(6): 539-543. DOI: 10.13374/j.issn1001-053x.1991.06.023
Citation: Sun Qingzu, Huang Yuanding, Yang Wangyue, Chen Guoliang. The Ductility of Fe3Al Intermetallic Compounds (I)[J]. Chinese Journal of Engineering, 1991, 13(6): 539-543. DOI: 10.13374/j.issn1001-053x.1991.06.023

Fe3Al金属间化合物的韧化(I)

The Ductility of Fe3Al Intermetallic Compounds (I)

  • 摘要: 通过加铬合金化及合理的热加工工艺,制得了高室温韧性Fe3Al金属间化合物。实验结果表明:合金元素铬的添加,改变了铁铝合金的断裂模式,即由纯解理断裂模式变为解理、沿晶混合断裂模式;铬的加入改善了室温韧性,提高了解理强度。

     

    Abstract: A Fe3Al intermetallic compound with high room temperature ductility has been obtained by means of combination of proper alloying addition and hot deformation. The relationship between properties and fractography was investigated. It was found that the fracture model of the alloys became a mired intergranuar-cleavage model while the Fe3Al containing no Cr showed pure cleavage one. The improvement of room ductility can be attributed to the increase of cleavage strength.

     

/