阮煦寰, 李伟, 王先进. 轧制工艺参数对1Cr13不锈钢成型性的影响[J]. 工程科学学报, 1992, 14(1): 56-62. DOI: 10.13374/j.issn1001-053x.1992.01.026
引用本文: 阮煦寰, 李伟, 王先进. 轧制工艺参数对1Cr13不锈钢成型性的影响[J]. 工程科学学报, 1992, 14(1): 56-62. DOI: 10.13374/j.issn1001-053x.1992.01.026
Ruan Xuhuan, Li Wei, Wang Xianjin. Effect of Cold Rolling Process on Basic Feature of Formablity of the 1Cr13 Stainless Steel Sheet[J]. Chinese Journal of Engineering, 1992, 14(1): 56-62. DOI: 10.13374/j.issn1001-053x.1992.01.026
Citation: Ruan Xuhuan, Li Wei, Wang Xianjin. Effect of Cold Rolling Process on Basic Feature of Formablity of the 1Cr13 Stainless Steel Sheet[J]. Chinese Journal of Engineering, 1992, 14(1): 56-62. DOI: 10.13374/j.issn1001-053x.1992.01.026

轧制工艺参数对1Cr13不锈钢成型性的影响

Effect of Cold Rolling Process on Basic Feature of Formablity of the 1Cr13 Stainless Steel Sheet

  • 摘要: 研究了冷轧工艺参数对1Cr13不锈钢薄板基本成型指标的影响,找出了影响其指标的重要因素:冷轧总压下率、退火温度。通过研究分析指出,适用于深拉成型1Cr13不锈钢的冷轧工艺参数为:冷轧总压下率60%,退火温度750℃,空冷。并从金相织构等方面对其机理进行了分析。

     

    Abstract: It has been found that main factors effecting on the forming property are the total reduction of cold rolling and the annealing temperature.The results obtained shows that optimum process parameters for deep drawing lCr13 stainless steel sheet are: the total ruduction is 60%,the annealing temperature is 750℃ followed with the air-cooling, The aspect of metallurgical structure and texlure was also discussed.

     

/