杨世山, 沈甦, 李治全, 曹永仙. 包头2号矿体选冶经济高效流程的开发[J]. 工程科学学报, 1995, 17(3): 218-223. DOI: 10.13374/j.issn1001-053x.1995.03.004
引用本文: 杨世山, 沈甦, 李治全, 曹永仙. 包头2号矿体选冶经济高效流程的开发[J]. 工程科学学报, 1995, 17(3): 218-223. DOI: 10.13374/j.issn1001-053x.1995.03.004
Yang Shishan, Shen Su, Li Zhiquan, Cao Yongxian. New Combined Process of Niobium Enrichment from No.2 Ore Body of Baotou Niobium-Bearing Iron Ore[J]. Chinese Journal of Engineering, 1995, 17(3): 218-223. DOI: 10.13374/j.issn1001-053x.1995.03.004
Citation: Yang Shishan, Shen Su, Li Zhiquan, Cao Yongxian. New Combined Process of Niobium Enrichment from No.2 Ore Body of Baotou Niobium-Bearing Iron Ore[J]. Chinese Journal of Engineering, 1995, 17(3): 218-223. DOI: 10.13374/j.issn1001-053x.1995.03.004

包头2号矿体选冶经济高效流程的开发

New Combined Process of Niobium Enrichment from No.2 Ore Body of Baotou Niobium-Bearing Iron Ore

  • 摘要: 采用包头2号矿体的重选粗精矿(含Nb2O51.6%~1.8%),用磁化焙烧-磁选,交流等离子冶炼工艺流程,可获得低磷中级铌铁(含铌22%~32%,Nb/P>30),铌收率61.l%.同时获得含铌铁精矿(TFe>60%,Nb2O5~1.0%),流程短效率高而经济。

     

    Abstract: A new combined magnetizing roasting-separation-smelting process of niobium enrichment from No.2 ore body of Baotou niobium-bearing iron ore has been developed. Using magnetizing roasting-magnetic separation-plasma smelting, a kind of middle grade ferroniobium of 22%~32% Nb and Nb/P>30 has been obtained and total niobium recovery ratio is 61.l%. This combined process has great economical potential because of its shorter flowsheet and more efficient operation.

     

/