强文江, 汤虹, 孙爱芝. HD处理烧结磁体制备各向异性NdFeB磁粉[J]. 工程科学学报, 2004, 26(3): 285-288. DOI: 10.13374/j.issn1001-053x.2004.03.015
引用本文: 强文江, 汤虹, 孙爱芝. HD处理烧结磁体制备各向异性NdFeB磁粉[J]. 工程科学学报, 2004, 26(3): 285-288. DOI: 10.13374/j.issn1001-053x.2004.03.015
QIANG Wenjiang, TANG Hong, SUN Aizhi. Manufacture of Anisotropic NdFeB Powders Process from Sintered Magnets by HD[J]. Chinese Journal of Engineering, 2004, 26(3): 285-288. DOI: 10.13374/j.issn1001-053x.2004.03.015
Citation: QIANG Wenjiang, TANG Hong, SUN Aizhi. Manufacture of Anisotropic NdFeB Powders Process from Sintered Magnets by HD[J]. Chinese Journal of Engineering, 2004, 26(3): 285-288. DOI: 10.13374/j.issn1001-053x.2004.03.015

HD处理烧结磁体制备各向异性NdFeB磁粉

Manufacture of Anisotropic NdFeB Powders Process from Sintered Magnets by HD

  • 摘要: 研究了通过吸氢破碎(HD)处理由烧结NdFeB磁体制取各向异性磁粉的方法.实验结果表明:HD处理温度是该处理过程中的关键参数,对于最终获得的各向异性磁粉的矫顽力具有显著的影响,同时HD处理温度的变化决定了烧结磁体破碎过程中的断裂方式.当HD处理温度为220℃时,磁体主要以沿晶断裂方式破碎,再经过950℃温度下的热处理,获得的各向异性磁粉的矫顽力达到490 kA/m.

     

    Abstract: A manufacture method of anisotropic NdFeB magnet powders was investigated from sintered bulk magnets by hydrogen decrepitation (HD process): it is found that HD temperature plays a very important role affecting the coercivity of the obtained magnetic powders evidently. This temperature determines the fracture way of bulk magnets during HD process as well. In intergranular fracture way through properly controlled HD temperature, at 220 ℃ for instance, anisotropic magnet powders with a coercivity up to 490 kA/m are obtained after a following annealing treatment at 950 ℃.

     

/