郝阳, 包燕平, 李任春, 李太全, 程迪, 陈霄, 王睿. 冶炼关键参数对于IF钢轧材夹杂缺陷的影响[J]. 工程科学学报, 2017, 39(3): 369-376. DOI: 10.13374/j.issn2095-9389.2017.03.008
引用本文: 郝阳, 包燕平, 李任春, 李太全, 程迪, 陈霄, 王睿. 冶炼关键参数对于IF钢轧材夹杂缺陷的影响[J]. 工程科学学报, 2017, 39(3): 369-376. DOI: 10.13374/j.issn2095-9389.2017.03.008
HAO Yang, BAO Yan-ping, LI Ren-chun, LI Tai-quan, CHENG Di, CHEN Xiao, WANG Rui. Influence of key parameters in steelmaking progress on the inclusion defects of rolled IF steel sheet[J]. Chinese Journal of Engineering, 2017, 39(3): 369-376. DOI: 10.13374/j.issn2095-9389.2017.03.008
Citation: HAO Yang, BAO Yan-ping, LI Ren-chun, LI Tai-quan, CHENG Di, CHEN Xiao, WANG Rui. Influence of key parameters in steelmaking progress on the inclusion defects of rolled IF steel sheet[J]. Chinese Journal of Engineering, 2017, 39(3): 369-376. DOI: 10.13374/j.issn2095-9389.2017.03.008

冶炼关键参数对于IF钢轧材夹杂缺陷的影响

Influence of key parameters in steelmaking progress on the inclusion defects of rolled IF steel sheet

  • 摘要: 针对邯钢IF钢冶炼过程,采用统计学软件SPSS中逻辑回归分析、相关性统计、描述性统计等方法,研究了冶炼过程中关键参数和轧材夹杂缺陷之间的对应关系以及参数间的相关性.结果表明:在IF钢冶炼过程中将转炉终点温度控制在1695~1700℃之间,吹氧量控制在250 m3以下,静置时间控制在30~40 min之间,加铝前氧位不超过3.9×10-4时,IF钢轧材出现夹杂缺陷的机率减少.由此对现场提出了改善措施,结果表明以上优化措施可以减少IF钢轧材中夹杂缺陷的产生.

     

    Abstract: Aiming at the steelmaking process of IF steel in Han-Steel, the relationship between key parameters and the defects of the rolled sheet was investigated, and the correlation among the parameters was also analyzed through the logic regression analysis, correlation statistics, descriptive statistics and other methods in the statistical software SPSS. The results show that the probability of inclusion defects in the rolled sheet reduces in the steelmaking process of IF steel when the end-point temperature of BOF is controlled in the range of 1695-1700℃, the oxygen blow amount below 250 m3, the holding time in the range of 30-40 min and the oxygen content before adding aluminum below 3. 9×10-4. Besides, the improvement measures were carried out and the results show that the optimization measures can reduce the inclusion defects of rolled IF steel sheet.

     

/