Tian Zhongzhuo, Lu Rongbang, Chang Xiangrong, Xiao Jimei, Feng Yifeng. The Relation Between Degssing Baking Treatment and Fracture Taughness of Cadmium-plated High-Strength Steel[J]. Chinese Journal of Engineering, 1984, 1(4): 71-80. DOI: 10.13374/j.issn1001-053x.1984.04.007
Citation: Tian Zhongzhuo, Lu Rongbang, Chang Xiangrong, Xiao Jimei, Feng Yifeng. The Relation Between Degssing Baking Treatment and Fracture Taughness of Cadmium-plated High-Strength Steel[J]. Chinese Journal of Engineering, 1984, 1(4): 71-80. DOI: 10.13374/j.issn1001-053x.1984.04.007

超高强钢的滞后破环

The Relation Between Degssing Baking Treatment and Fracture Taughness of Cadmium-plated High-Strength Steel

  • 摘要: 用WOL和悬臂梁试样研究了高强度镀镉钢35℃rMnSiA,并确定了钢中和镀层中的氢量。镀层富氢,在200℃通过光亮,致密镀层脱氢很慢,钢中氢量起初升高,2—2.5小时后达到峰值,然后下降。钢的滞后破坏性能取决于钢中氢量,当钢中氢量达到峰值时,其KISCC最小,da/dt最大。为了提高武器质量,有必要延长脱氢时间。

     

    Abstract: The cadmium plated high-strength steel 35CrMnSiA was studied using modified WOL and cantilever beam specimens.The hydrogen content in cadmium coating was determined as well as the content in steel. The cadmium plating is enriched with hydrogen.The degassing at 200℃ through bright, nonporous coating is very slow.Hydrogen content in the steel increases first during baking and reaches its maximum at about 2-2.5 hours, then decreases slawly.The delayed fracture properties of the steel depend on its hydrogen content.When the hydrogen content in steel is at its maximum, the KIscc of the steel reaches its minimum and da/dt reachs its maximum.In order to improve the mechanical prorepties, its necessary to take a prolonged degassing baking treatment.

     

/