陈伟庆, 周荣章, 林宗彩. Equilibrium between Slag and Molten Iron in the Direct Alloying of Steel with Nb2O5-Bearing Slag[J]. 工程科学学报, 1989, 11(6): 526-532. DOI: 10.13374/j.issn1001-053x.1989.06.023
引用本文: 陈伟庆, 周荣章, 林宗彩. Equilibrium between Slag and Molten Iron in the Direct Alloying of Steel with Nb2O5-Bearing Slag[J]. 工程科学学报, 1989, 11(6): 526-532. DOI: 10.13374/j.issn1001-053x.1989.06.023
Chen Weiqing, Zhou Rongzhang, Lin Zongcai. Equilibrium between Slag and Molten Iron in the Direct Alloying of Steel with Nb2O5-Bearing Slag[J]. Chinese Journal of Engineering, 1989, 11(6): 526-532. DOI: 10.13374/j.issn1001-053x.1989.06.023
Citation: Chen Weiqing, Zhou Rongzhang, Lin Zongcai. Equilibrium between Slag and Molten Iron in the Direct Alloying of Steel with Nb2O5-Bearing Slag[J]. Chinese Journal of Engineering, 1989, 11(6): 526-532. DOI: 10.13374/j.issn1001-053x.1989.06.023

Equilibrium between Slag and Molten Iron in the Direct Alloying of Steel with Nb2O5-Bearing Slag

Equilibrium between Slag and Molten Iron in the Direct Alloying of Steel with Nb2O5-Bearing Slag

  • 摘要: Equilibrium between slag and molten iron at 1600℃ was investigated for the direct alloying of steel with Nb2O6-bearing slag. The activity of niobium oxide in the slag was measured. The αNb2O5 is in the range of 10-2-10-4. TheδNb2O5 is ranged in 100-10-2.Niobium partition decreases with the increase ofSi% and CaO/SiO2. When α0 and ΣFeO decrease, niobium partition decreases too. The δNb2o5 and the ratio of γsiO2 to γNb2O5 decrease with the incre-ase of slag basicity. The suitable thermodynamic conditions in direct alloying of steel with Nb2O5-bearing slag have been found.

     

    Abstract: Equilibrium between slag and molten iron at 1600℃ was investigated for the direct alloying of steel with Nb2O6-bearing slag. The activity of niobium oxide in the slag was measured. The αNb2O5 is in the range of 10-2-10-4. TheδNb2O5 is ranged in 100-10-2.Niobium partition decreases with the increase ofSi% and CaO/SiO2. When α0 and ΣFeO decrease, niobium partition decreases too. The δNb2o5 and the ratio of γsiO2 to γNb2O5 decrease with the incre-ase of slag basicity. The suitable thermodynamic conditions in direct alloying of steel with Nb2O5-bearing slag have been found.

     

/