赵爱民, 王兆昌. 加筋复合白口铁的强韧化及断裂方式[J]. 工程科学学报, 1991, 13(2): 123-129. DOI: 10.13374/j.issn1001-053x.1991.02.005
引用本文: 赵爱民, 王兆昌. 加筋复合白口铁的强韧化及断裂方式[J]. 工程科学学报, 1991, 13(2): 123-129. DOI: 10.13374/j.issn1001-053x.1991.02.005
Zhao Aimin, Wang Zhaochang. Strengthening, Toughening and Fracture Behavior of Composite White Cast Iron[J]. Chinese Journal of Engineering, 1991, 13(2): 123-129. DOI: 10.13374/j.issn1001-053x.1991.02.005
Citation: Zhao Aimin, Wang Zhaochang. Strengthening, Toughening and Fracture Behavior of Composite White Cast Iron[J]. Chinese Journal of Engineering, 1991, 13(2): 123-129. DOI: 10.13374/j.issn1001-053x.1991.02.005

加筋复合白口铁的强韧化及断裂方式

Strengthening, Toughening and Fracture Behavior of Composite White Cast Iron

  • 摘要: 研究了加筋式复合白口铁的机械性能、强韧化机理及其断裂方式。实验结果表明:加筋复合白口铁的机械性能优于单一的白口铁,其抗弯强度及冲击韧性随钢筋的体积分数的增加而增加,在合适的钢筋体积分数时强韧化效果最好。对复合白口铁的冲击试样的断口进行SEM观察,发现复合白口铁中钢筋有3种断裂方式,即完全脆性断裂、部分脆性断裂和韧性断裂,它们影响复合白口铁的强度和冲击韧性。

     

    Abstract: The strengthening, toughening and fracture behavior of composite white cast iron which was composed of reinforcement steel bar and white cast iron have been researched. The results of bend tests and impact tests of specimens of composite white cast iron indicated that the bending strength and impact toughness of it were superior to those of straight white cast iron. The improvements of bending strength and impact toughness were related to the volume fraction of reinforcement bar. Three fracture modes of steel bar in composite white cast iron were found by examining the surfaces of fracture by SEM. Those were brittle fracture, ductile fracture and mixed fra- cture, and thus the different strength and toughness of composite white cast iron were effected.

     

/