易秉钺, 陈键, 周建梁. 20CrMnMo渗碳淬火齿轮的接触疲劳强度[J]. 工程科学学报, 1992, 14(5): 530-536. DOI: 10.13374/j.issn1001-053x.1992.05.007
引用本文: 易秉钺, 陈键, 周建梁. 20CrMnMo渗碳淬火齿轮的接触疲劳强度[J]. 工程科学学报, 1992, 14(5): 530-536. DOI: 10.13374/j.issn1001-053x.1992.05.007
Yi Bingyue, Chen Jian, Zhou Jianliang. Contact Fatigue Strength of 20CrMnMo Carburized and Quenched Gears[J]. Chinese Journal of Engineering, 1992, 14(5): 530-536. DOI: 10.13374/j.issn1001-053x.1992.05.007
Citation: Yi Bingyue, Chen Jian, Zhou Jianliang. Contact Fatigue Strength of 20CrMnMo Carburized and Quenched Gears[J]. Chinese Journal of Engineering, 1992, 14(5): 530-536. DOI: 10.13374/j.issn1001-053x.1992.05.007

20CrMnMo渗碳淬火齿轮的接触疲劳强度

Contact Fatigue Strength of 20CrMnMo Carburized and Quenched Gears

  • 摘要: 对齿面硬度HRC62的20CrMnMo渗碳淬火齿轮,进行了接触疲劳运转试验,获得33个试验数据。经过数据处理,绘制出R-S-N曲线,可靠度0.99,循环基数5×107,其齿面接触疲劳极限应力为1571.6N/mm2。通过电镜等,对齿面损伤特性进行了宏观和微观的分析,获得一些有益的观点,提出一些有效的技术措施。

     

    Abstract: Using power circulating type gear tester, 33 pairs 20CrMnMo carburized and quenched gears, having tooth surface hardness HRC62, were tested to investigate the contact fatigue life. The test results were treated by statistical methods and plotted as R-S-N curve. The contact strength limits σHlim were 1 571.6 N/mm2 with reliability 0.99 at 5×107 cystes. By using scanning electron microscope etc., the texture of tooth surface damage were described and the mechanism of failures was investigated.

     

/