周寿增, 梅武, 唐伟忠, 史振华. 铸态Tb0.27Dy0.73Fex合金的组织与磁特性[J]. 工程科学学报, 1993, 15(2): 159-163. DOI: 10.13374/j.issn1001-053x.1993.02.006
引用本文: 周寿增, 梅武, 唐伟忠, 史振华. 铸态Tb0.27Dy0.73Fex合金的组织与磁特性[J]. 工程科学学报, 1993, 15(2): 159-163. DOI: 10.13374/j.issn1001-053x.1993.02.006
Zhou Shouzeng, Mei Wu, Tang Weizhong, Shi Zhenhua. Magnetostrictive Properties and Microstructure of Tb0.27Dy0.73Fex Alloys in as-Cast[J]. Chinese Journal of Engineering, 1993, 15(2): 159-163. DOI: 10.13374/j.issn1001-053x.1993.02.006
Citation: Zhou Shouzeng, Mei Wu, Tang Weizhong, Shi Zhenhua. Magnetostrictive Properties and Microstructure of Tb0.27Dy0.73Fex Alloys in as-Cast[J]. Chinese Journal of Engineering, 1993, 15(2): 159-163. DOI: 10.13374/j.issn1001-053x.1993.02.006

铸态Tb0.27Dy0.73Fex合金的组织与磁特性

Magnetostrictive Properties and Microstructure of Tb0.27Dy0.73Fex Alloys in as-Cast

  • 摘要: 研究了铸态Tb0.27Dy0.73Fex(x=1.65~2.0)化合物的磁致伸缩特性,显微组织与Fe含量x之间的相互关系规律。当x=19时,铸态的λ11、λ11-λ和(dλ/dH)m具有最大值。该合金的第二相数量最少,单相性较好。基体相Tb0.27Dy0.73Fe2.0具有MgCu2型结构。当x ≥ 1.95时,合金出现RFe3相魏氏体组织,贯穿基体相晶粒,导至磁致伸缩特性下降。当x ≤ 1.85时,合金出现网络状的离异共晶组织和鱼骨状的共晶组织。随x的降低,共晶相数量增加并粗化,从而导致磁致伸缩特性下降。

     

    Abstract: The relations between the magnetostrictive properties and microstructure, iron content.x of the alloy Tb0.27Dy0.73Fex(x=1.65-2.0) in as-cast have been studied. The matrix phase of this alloy has MgCu2 type structure. When x=1.90, the alloy in as-cast with small amount of second phase possesses a maximum values of λ1111-λ and (dλ/dH)m. When x is equal to or large than 1.95, the RFe3 phase with Widmantanten-type morphology apppears, which leads to the decrease of magnetostrictive properties of the alloys. When iron content x is less than or equal to 1.85, the divorce eutectic structure or the two eutectic structure is observed, which causes the drop of the magnetostrictive properties of the alloys.

     

/