李宏, 王万军, 李景捷, 王欣, 周荣章. 红热钒渣吹氧氧化后碱浸提钒[J]. 工程科学学报, 1994, 16(1): 14-19. DOI: 10.13374/j.issn1001-053x.1994.01.004
引用本文: 李宏, 王万军, 李景捷, 王欣, 周荣章. 红热钒渣吹氧氧化后碱浸提钒[J]. 工程科学学报, 1994, 16(1): 14-19. DOI: 10.13374/j.issn1001-053x.1994.01.004
Li Hong, Wang Wanjun, Li Jingjie, Wang Xin, Zhou Rongzhang. Extracting Vanadium with Alkaline Leaching after Blowing Oxygen to Hot Vanadium Slag[J]. Chinese Journal of Engineering, 1994, 16(1): 14-19. DOI: 10.13374/j.issn1001-053x.1994.01.004
Citation: Li Hong, Wang Wanjun, Li Jingjie, Wang Xin, Zhou Rongzhang. Extracting Vanadium with Alkaline Leaching after Blowing Oxygen to Hot Vanadium Slag[J]. Chinese Journal of Engineering, 1994, 16(1): 14-19. DOI: 10.13374/j.issn1001-053x.1994.01.004

红热钒渣吹氧氧化后碱浸提钒

Extracting Vanadium with Alkaline Leaching after Blowing Oxygen to Hot Vanadium Slag

  • 摘要: 红热钒渣吹氧氧化仅10min左右,经碱浸压煮提钒,钒浸出率可达90%以上.吹氧过程中,增添CaO,控制合适的MgO与钒渣的重量比,减小供氧速率,可获得高的CFe3+/CFe2+.碱浸时,钒浸出率主要随CFe3+/CFe2+的增大而升高.保温时间、浸出温度、Na2CO3和NaOH的加入比、渣水质量比对钒浸出率都有影响.碱浸压煮时充氧和水洗残渣也可以提高钒的总浸出率.

     

    Abstract: The hot V slag were first oxidized ouly 10 odd min.with blowing oxygen and then were alkaline leached,the leaching ratio of V come up to 90%.Higher CFe3+/CFe2+ can be obtained in case of increasing the addition of CaO into V slag,weight ratio of MgO and slag is controlled in optimum range, and decreasing the rate of oxygen supply in blowing oxygen process,Leaching ratio of V increases major with the increases of CFe3+/CFe2+. Holding time,leaching temperature,the addition ratio of Na2CO3,and NaOH,and the weight ratio of slag and water influence the leaching ratio of V.The total leaching ratio of V increases with the oxygenation during V slag alkaline autoclave leaching and during residuel slag water leaching.

     

/