杨志尚, 章复中, 任立斌, 周荣章, 余宗森. 添加钇对TiAl合金组织和性能的影响[J]. 工程科学学报, 1995, 17(5): 424-428. DOI: 10.13374/j.issn1001-053x.1995.05.005
引用本文: 杨志尚, 章复中, 任立斌, 周荣章, 余宗森. 添加钇对TiAl合金组织和性能的影响[J]. 工程科学学报, 1995, 17(5): 424-428. DOI: 10.13374/j.issn1001-053x.1995.05.005
Yang Zhishang, Zhang Fuzhong, Ren Libin, Zhou Rongzhang, Yu Zongsen. Effects of Y-Addition on Microstructure and Mechanical Properties of TiAl -Base Alloys[J]. Chinese Journal of Engineering, 1995, 17(5): 424-428. DOI: 10.13374/j.issn1001-053x.1995.05.005
Citation: Yang Zhishang, Zhang Fuzhong, Ren Libin, Zhou Rongzhang, Yu Zongsen. Effects of Y-Addition on Microstructure and Mechanical Properties of TiAl -Base Alloys[J]. Chinese Journal of Engineering, 1995, 17(5): 424-428. DOI: 10.13374/j.issn1001-053x.1995.05.005

添加钇对TiAl合金组织和性能的影响

Effects of Y-Addition on Microstructure and Mechanical Properties of TiAl -Base Alloys

  • 摘要: 设计并熔炼了成分为(Ti50Al50)100-xYx(x(atom)=0~2.0%)的合金,用金相显微镜、扫描电镜、三点弯曲试验等手段,研究了添加钇(Y)对TiAl合金显微组织和力学性能的影响。结果表明:钇的添加能改变TiAl合金显微组织,使γTiAl合金晶粒细化,促进γ+α2片层状组织的形成。适量钇的添加能降低TiAl合金中O、N等间隙原子含量并增加TiAl合金的室温抗弯强度和塑性;当钇的添加量超过其在TiAl合金中的固溶度时,将形成新的Ti-Al-Y三元化合物,反而会降低TiAl合金的室温强度和塑性。

     

    Abstract: (Ti50Al50)100-xYx ternary alloys with various Y content(x(atom)=0~2.0%) were designed and smelt.The effect of Y-addition on microstructure and mechanieal properties of TiAl alloys are investigated by metallography,scanning electron microscope,3-point bending tests and so on.The results show that the Y-addition can change the microstructure of TiAl alloys such as fining the grain size of γTiAl and promoting the formation of γ+α2 lammellar structure;Y in suitable addition amount can absorb interetitial atoms such as O and N and improve strength and ductility of TiAl alloys at ambient temperature;The strength and ductility of TiAl alloys will decrease because of the formation of new ternary compounds when Y-addition amount exceeds its solid solubility in TiAl alloys.

     

/