胡小华, 陈国良, 杨王玥, 许嘉龙. Ti-12Co-5Al合金的βα+Ti2Co时效相变与硬度[J]. 工程科学学报, 1998, 20(6): 536-540. DOI: 10.13374/j.issn1001-053x.1998.06.007
引用本文: 胡小华, 陈国良, 杨王玥, 许嘉龙. Ti-12Co-5Al合金的βα+Ti2Co时效相变与硬度[J]. 工程科学学报, 1998, 20(6): 536-540. DOI: 10.13374/j.issn1001-053x.1998.06.007
Hu Xiaohua, Chen Guoliang, Yang Wangyue, Xu Jialong. Aging Procedure and Its Hardness Change from Single β-Ti Phase to α+Ti2Co Dual Phase of Alloy Ti-12Co-5Al[J]. Chinese Journal of Engineering, 1998, 20(6): 536-540. DOI: 10.13374/j.issn1001-053x.1998.06.007
Citation: Hu Xiaohua, Chen Guoliang, Yang Wangyue, Xu Jialong. Aging Procedure and Its Hardness Change from Single β-Ti Phase to α+Ti2Co Dual Phase of Alloy Ti-12Co-5Al[J]. Chinese Journal of Engineering, 1998, 20(6): 536-540. DOI: 10.13374/j.issn1001-053x.1998.06.007

Ti-12Co-5Al合金的βα+Ti2Co时效相变与硬度

Aging Procedure and Its Hardness Change from Single β-Ti Phase to α+Ti2Co Dual Phase of Alloy Ti-12Co-5Al

  • 摘要: 研究了超塑合金Ti-12Co-5Al非平衡态β相α+Ti2Co共析转变的时效过程以及它的硬度变化。当温度为450℃时,随着时间的增长硬度随之增加,β相的转变也更加完全,转变产物之间以及转变产物与母相之间的相变也从完全共格到半共格再到完全非共格,而峰值发生在320min左右;当时间为20min时,随温度的升高也具有相同的规律,峰值发生在600℃左右。Al元素除了具有固溶强化的作用之外,还有提高共析相变温度,从而减缓了相转变动力学的进行。

     

    Abstract: Ageing process and its hardness change from β to α+Ti2Co of alloy Ti-12Co-5Al were investigated. At 450℃,the amount of transformation increases with ageing time and the boundary between the transformation product and the matrix changes from coherent to incoherent. The maximum hardness is achieved at around 320 minutes. With the same ageing time of 20 minutes, the same thing happens as above with increasing temperatures and the hardness peaks at around 600℃.The addition of element aluminum slows down the kinetics of ageing transformation in addition to its strengthening effect.

     

/