刘学华, 韩传基, 蔡开科, 宋超, 茆勇, 孙维, 张建平. 小方坯连铸低碳低硅铝镇静钢可浇性[J]. 工程科学学报, 2005, 27(4): 431-435. DOI: 10.13374/j.issn1001-053x.2005.04.011
引用本文: 刘学华, 韩传基, 蔡开科, 宋超, 茆勇, 孙维, 张建平. 小方坯连铸低碳低硅铝镇静钢可浇性[J]. 工程科学学报, 2005, 27(4): 431-435. DOI: 10.13374/j.issn1001-053x.2005.04.011
LIU Xuehua, HAN Chuanji, CAI Kaike, SONG Chao, MAO Yong, SUN Wei, ZHANG Jianping. Castability of billet continuous casting for low-carbon low-silicon Al-killed steel[J]. Chinese Journal of Engineering, 2005, 27(4): 431-435. DOI: 10.13374/j.issn1001-053x.2005.04.011
Citation: LIU Xuehua, HAN Chuanji, CAI Kaike, SONG Chao, MAO Yong, SUN Wei, ZHANG Jianping. Castability of billet continuous casting for low-carbon low-silicon Al-killed steel[J]. Chinese Journal of Engineering, 2005, 27(4): 431-435. DOI: 10.13374/j.issn1001-053x.2005.04.011

小方坯连铸低碳低硅铝镇静钢可浇性

Castability of billet continuous casting for low-carbon low-silicon Al-killed steel

  • 摘要: 在分析水口堵塞的基础上,结合马钢三炼钢生产实际,采用正交实验法研究了钙处理的喂线速度、喂线量和中间包水口内径对140mm×140mm小方坯连铸低碳低硅高酸溶铝钢水口堵塞的影响.结果表明,提高喂线速度、加大喂线量和增加水口内径可避免水口的堵塞.采用以上工艺,连浇炉数达8~10炉,且铸坯内部和表面质量良好.

     

    Abstract: On the basis of analyzing nozzle clogging, the effects of feeding speed, the amount of Ca-Fe cored wire during Ca-treatment and nozzle diameter on the castablity of billet continuous casting for low-carbon low-silicon Al-killed steel were studied by an orthogonal test in line with the on-site condition of No.3 Steelmaking Shop of Ma-Steel, China. The results showed that increasing the feeding speed, the amount of Ca-Fe cored wire and the diameter of the tundish nozzle can prevent blockage. After adopting these parameters proposed, 8-10 heats could be cast in sequence, and the surface quality and internal quality of the billets are satisfactory.

     

/