LIU Rong, RU Hongqiang, ZHAO Yuan, TANG Di. Preparation process of ZrB2/B4C ceramic composites by pressureless sintering based on mechanical mixing[J]. Chinese Journal of Engineering, 2006, 28(8): 762-765. DOI: 10.13374/j.issn1001-053x.2006.08.012
Citation: LIU Rong, RU Hongqiang, ZHAO Yuan, TANG Di. Preparation process of ZrB2/B4C ceramic composites by pressureless sintering based on mechanical mixing[J]. Chinese Journal of Engineering, 2006, 28(8): 762-765. DOI: 10.13374/j.issn1001-053x.2006.08.012

基于机械混合法无压烧结制备ZrB2/B4C陶瓷复合材料

Preparation process of ZrB2/B4C ceramic composites by pressureless sintering based on mechanical mixing

  • 摘要: 研究无压烧结条件下原位合成工艺对ZrB2/B4C陶瓷复合材料的烧结致密化、力学性能、显微组织的影响.结果表明材料的密度随着烧结温度的增加和保温时间的延长先增加后降低,在烧结温度2060℃,保温30min时,ZrB2/B4C复合材料的相对密度可达93.2%;材料的硬度随着温度的升高而增大,在2070℃时达到最大值;材料的断裂韧性则随着温度的升高呈现下降趋势,从2000℃时的4.04MPa·m1/2下降到2060℃时的2.36MPa·m1/2.

     

    Abstract: This paper investigated the effects of pressureless sintering in suit synthesis process on the density, physical properties and microstructure of ZrB2/B4C ceramic composites. The results showed that, as the sintering temperature increasing and the holding time extending, the density increased first and then decreased, and the maximum relative density of the composites synthesized at 2 060℃for 30 min was 93.2%; the hardness rised with increasing temperature and its value reached to the peak at 2 070℃; opposite to the hardness, the fracture toughness decreased from 4.04 MPa·m1/2 at 2 000℃ to 2.36 MPa·m1/2 at 2 060℃.

     

/