季春生, 王忠诚, 刘剑辉. 改善20CrMnTiH淬透性的研究[J]. 工程科学学报, 2007, 29(S1): 85-88. DOI: 10.13374/j.issn1001-053x.2007.s1.025
引用本文: 季春生, 王忠诚, 刘剑辉. 改善20CrMnTiH淬透性的研究[J]. 工程科学学报, 2007, 29(S1): 85-88. DOI: 10.13374/j.issn1001-053x.2007.s1.025
JI Chunsheng, WANG Zhongcheng, LIU Jianhui. Study of narrow hardenability bands of 20CrMnTiH[J]. Chinese Journal of Engineering, 2007, 29(S1): 85-88. DOI: 10.13374/j.issn1001-053x.2007.s1.025
Citation: JI Chunsheng, WANG Zhongcheng, LIU Jianhui. Study of narrow hardenability bands of 20CrMnTiH[J]. Chinese Journal of Engineering, 2007, 29(S1): 85-88. DOI: 10.13374/j.issn1001-053x.2007.s1.025

改善20CrMnTiH淬透性的研究

Study of narrow hardenability bands of 20CrMnTiH

  • 摘要: 莱钢特钢厂20CrMnTiH钢材成分波动较大,淬透性带HRC8~10,范围较大,制约了齿轮钢质量的进一步提高.通过研究,发现铸坯中心偏析尤其是碳偏析为主要问题.通过工艺优化采取各项措施,尤其增加电磁搅拌后,中心碳偏析得到明显改善;C控制在0.19%~0.20%的炉次达到了95.6%;淬透性带控制在HRC6内的达到了92.1%;在HRC4内的达到了86.2%;提高了产品质量,满足了用户需求.

     

    Abstract: The component fluctuation of 20CrMnTiH steel in Laiwu Special Steel Plant was large,the-hardenability bands belt was HRC 8-10,this constrained the further improvement of gear steel quality.Based on the research,it was found that center segregation especially carbon segregation in blooms was the major prob-lem.By taking measures,especially the increase of electromagnetic stirring,the center carbon segregation was markedly improved;C control between 0.19%~0.22% reached 95.6%;hardenability bands belt control in HRC 6 reached 92.1% and in HRC 4 reached 86.2%.The quality of products is improved and the needs of users are met.

     

/

返回文章