王谦, 何生平, 解丹, 黄青云, Z. S. LI, K. C. MILLS. 低碳钢板坯连铸用无氟保护渣生成区域的研究[J]. 工程科学学报, 2008, 30(5): 487-491. DOI: 10.13374/j.issn1001-053x.2008.05.010
引用本文: 王谦, 何生平, 解丹, 黄青云, Z. S. LI, K. C. MILLS. 低碳钢板坯连铸用无氟保护渣生成区域的研究[J]. 工程科学学报, 2008, 30(5): 487-491. DOI: 10.13374/j.issn1001-053x.2008.05.010
WANG Qian, HE Shengping, XIE Dan, HUANG Qingyun, Z. S. LI, K. C. MILLS. Formation zone of fluorine-free mold fluxes for slab continuous casting of low carbon steel[J]. Chinese Journal of Engineering, 2008, 30(5): 487-491. DOI: 10.13374/j.issn1001-053x.2008.05.010
Citation: WANG Qian, HE Shengping, XIE Dan, HUANG Qingyun, Z. S. LI, K. C. MILLS. Formation zone of fluorine-free mold fluxes for slab continuous casting of low carbon steel[J]. Chinese Journal of Engineering, 2008, 30(5): 487-491. DOI: 10.13374/j.issn1001-053x.2008.05.010

低碳钢板坯连铸用无氟保护渣生成区域的研究

Formation zone of fluorine-free mold fluxes for slab continuous casting of low carbon steel

  • 摘要: 为了研究性能稳定的低碳钢板坯连铸用无氟保护渣,在测试传统的板坯连铸用高氟保护渣(F- ≥ 3%)性能的基础上,采用单纯形法,设计了CaO-SiO2-Al2O3-Fe2O3-MgO-Li2O-TiO2-Na2O-MnO-B2O3渣系中满足保护渣组成条件的基本实验点.通过逐步固定各组分含量,将多维空间的渣系组成转化为二维平面网格.测试无氟渣样的熔点、黏度、转折温度、玻璃体比例及转折温度时的黏度,并作性能与组成关系的等值线图.通过比较高氟保护渣和无氟渣样性能,确定了碱度、熔点、黏度、转折温度较低,且凝固后呈玻璃体的低碳钢板坯连铸用无氟保护渣的三个生成区域,其中之一的典型成分的质量分数范围是:CaO 31.2%,SiO2 36.8%,Al2O3 3%,Fe2O3 1%,MgO 2%,Li2O 2%,TiO2 6%,Na2O 7%~12%,MnO 3%~8%,B2O3 0~3%.

     

    Abstract: In order to develop fluorine-free mold fluxes into stable properties for slab continuous casting of low carbon steel, the formation regions of fluorine-free mold fluxes were investigated. Based on the test of the physical properties of traditional fluorine containing (F- ≥ 3%) fluxes, the slag samples, fitting to the compositional characteristics of mold fluxes, were designed by using the mathematical complex method in the slag system of CaO-SiO2-Al2O3-Fe2O3-MgO-Li2O-TiO2-Na2O-MnO-B2O3. By fixing some variable components step by step, the multidimensional composition space was transformed into two-dimensional plain grids, from which the nodal points were used as compositions of fluxes. Compared with the properties of fluorine containing fluxes, three formation regions of fluorine-free fluxes, with a lower basicity, melting point, viscosity and breaking temperature, and solidified in the glassy state, were found. The typical components in one of the regions were CaO 31.2%, SiO2 36.8%, Al2O3 3%, Fe2O3 1%, MgO 2%, Li2O 2%, TiO2 6%, Na2O 7%-12%, MNO 3%-8%, and B2O3 0-3%.

     

/