黎先浩, 康永林, 陈林恒, 焦国华, 温德智. CSP生产600MPa级低碳贝氏体钢的相变[J]. 工程科学学报, 2009, 31(6): 701-707. DOI: 10.13374/j.issn1001-053x.2009.06.016
引用本文: 黎先浩, 康永林, 陈林恒, 焦国华, 温德智. CSP生产600MPa级低碳贝氏体钢的相变[J]. 工程科学学报, 2009, 31(6): 701-707. DOI: 10.13374/j.issn1001-053x.2009.06.016
LI Xian-hao, KANG Yong-lin, CHEN Lin-heng, JIAO Guo-hua, WEN De-zhi. Continuous cooling transformation of 600 MPa grade low carbon bainite steel produced by CSP process[J]. Chinese Journal of Engineering, 2009, 31(6): 701-707. DOI: 10.13374/j.issn1001-053x.2009.06.016
Citation: LI Xian-hao, KANG Yong-lin, CHEN Lin-heng, JIAO Guo-hua, WEN De-zhi. Continuous cooling transformation of 600 MPa grade low carbon bainite steel produced by CSP process[J]. Chinese Journal of Engineering, 2009, 31(6): 701-707. DOI: 10.13374/j.issn1001-053x.2009.06.016

CSP生产600MPa级低碳贝氏体钢的相变

Continuous cooling transformation of 600 MPa grade low carbon bainite steel produced by CSP process

  • 摘要: 以低碳Nb、V、Ti、Mo和Cr合金化贝氏体钢为研究对象,在Formaster-Digital膨胀仪上测定了过冷奥氏体的静态CCT曲线;在Gleeble-1500热/力模拟机上,用膨胀法测定了奥氏体的动态CCT曲线;采用扫描电镜和透射电镜分析了贝氏体钢的室温组织演变规律.结果表明:合金元素抑制奥氏体向铁素体转变,在冷却速度大于10℃·s-1的范围内,静态CCT和动态CCT的室温组织均为贝氏体,具有较高的强度;奥氏体变形促进了贝氏体转变,贝氏体转变开始温度为610~668℃,终了温度为520~551℃.

     

    Abstract: The static and dynamic CCT curves of low carbon bainite steel microalloyed with Nb, V, Ti, Mo and Cr were tested with a Formaster-Digital dilatometer and a Gleeble-1500 thermo-mechanical simulator, respectively. The transformation microstructures were observed by SEM and TEM. It is shown that the transformation microstructures are bainite after continuous cooling when the cooling rate is more than 10℃·s-1 due to the fact that alloy additions inhibit the transformation from austenite to ferrite, which results in excellent strength; in addition, deformation promotes bainite transformation, and the start temperature and final temperature of bainite transformation are 610 to 668℃ and 520 to 551℃, respectively.

     

/