崔衡, 董志平, 时颜林, 李实, 杜建新, 刘竑, 包燕平. 含氮316L不锈钢氮合金化工艺研究[J]. 工程科学学报, 2009, 31(S1): 67-71. DOI: 10.13374/j.issn1001-053x.2009.s1.028
引用本文: 崔衡, 董志平, 时颜林, 李实, 杜建新, 刘竑, 包燕平. 含氮316L不锈钢氮合金化工艺研究[J]. 工程科学学报, 2009, 31(S1): 67-71. DOI: 10.13374/j.issn1001-053x.2009.s1.028
CUI Heng, DONG Zhi-ping, SHI Yan-lin, LI Shi, DU Jian-xin, LIU Hong, BAO Yan-ping. Study on the nitrogen alloying process of nitrogen-contained 316 L stainless steel[J]. Chinese Journal of Engineering, 2009, 31(S1): 67-71. DOI: 10.13374/j.issn1001-053x.2009.s1.028
Citation: CUI Heng, DONG Zhi-ping, SHI Yan-lin, LI Shi, DU Jian-xin, LIU Hong, BAO Yan-ping. Study on the nitrogen alloying process of nitrogen-contained 316 L stainless steel[J]. Chinese Journal of Engineering, 2009, 31(S1): 67-71. DOI: 10.13374/j.issn1001-053x.2009.s1.028

含氮316L不锈钢氮合金化工艺研究

Study on the nitrogen alloying process of nitrogen-contained 316 L stainless steel

  • 摘要: 在常压和真空条件下研究了温度与氮分压对316L不锈钢中氮溶解度的影响,钢中氮的溶解度随着温度的降低而升高,随着氮分压的增大而增大.建立了316L不锈钢氮溶解度热力学计算模型,不同吹氮条件下氮溶解度实测值与热力学模型计算值较吻合.在1773~1873K条件下,生产控氮型316L不锈钢,氮分压要控制在6~28kPa以上;生产中氮型316L不锈钢,氮分压要控制在22~101kPa以上.常压下吹氮10min,钢液含氮量即可超过0.10%.

     

    Abstract: The influences of liquid steel temperature and nitrogen partial pressure on the nitrogen solubility in 316 L stainless steel under normal atmosphere and vacuum were studied. The nitrogen solubility increased with decreasing the liquid steel temperature or increasing the nitrogen partial pressure. A thermodynamic model was developed to calculate the nitrogen solubility in 316 L stainless steel, and the calculated results were in coincidence with the measurement results under different nitrogen blowing processes. At 1 773 to 1 873 K, the nitrogen partial pressure must be over 6-28 kPa to produce 316LN (N:0.05%-0.10%, mass fraction, so as the follows), and must be over 22-101 kPa to produce 316 LN (N:0.10%-0.40%). The nitrogen content was over 0.01% in the condition of nitrogen blowing for 10 min under normal atmosphere.

     

/