胡昌旭, 倪东惠, 郑军君, 肖志瑜, 李元元. 流动温压成型铁基粉末冶金复杂件的脱脂工艺[J]. 工程科学学报, 2010, 32(3): 336-339. DOI: 10.13374/j.issn1001-053x.2010.03.017
引用本文: 胡昌旭, 倪东惠, 郑军君, 肖志瑜, 李元元. 流动温压成型铁基粉末冶金复杂件的脱脂工艺[J]. 工程科学学报, 2010, 32(3): 336-339. DOI: 10.13374/j.issn1001-053x.2010.03.017
HU Chang-xu, NI Dong-hui, ZHENG Jun-jun, XIAO Zhi-yu, LI Yuan-yuan. Degreasing behavior of iron-based powder metallurgy complex parts by warm flow compaction[J]. Chinese Journal of Engineering, 2010, 32(3): 336-339. DOI: 10.13374/j.issn1001-053x.2010.03.017
Citation: HU Chang-xu, NI Dong-hui, ZHENG Jun-jun, XIAO Zhi-yu, LI Yuan-yuan. Degreasing behavior of iron-based powder metallurgy complex parts by warm flow compaction[J]. Chinese Journal of Engineering, 2010, 32(3): 336-339. DOI: 10.13374/j.issn1001-053x.2010.03.017

流动温压成型铁基粉末冶金复杂件的脱脂工艺

Degreasing behavior of iron-based powder metallurgy complex parts by warm flow compaction

  • 摘要: 使用水雾化铁粉等原料制备十字形试样,对脱脂工艺、微观组织进行了分析,得到的理想脱脂工艺为:先以较快的速率升温到160℃,然后以1℃·min-1的速率升温到300℃,保温0.5h,再以1.5℃·min-1的速率升温到450℃,保温0.5h.烧结在1300℃进行.实验结果表明,通过优化脱脂工艺,使用流动温压工艺,可以制备出成本低廉、形状复杂的结构件.

     

    Abstract: Water-atomized iron powders were used by warm flow compaction to fabricate cross-shaped parts.The degrease process and microstructure of sintered parts were investigated.The optimal degrease process is to raise the temperature from ambient temperature to 160 ℃,then raise to 300 ℃ at a rate of 1 ℃·min-1 and hold at 300 ℃ for 0.5 h,followed by raising the temperature to 450 ℃ at a rate of 1.5 ℃·min-1 and hold at 450 ℃ for 0.5 h.Sintering was carried out at 1 300 ℃.It is shown that at the proper degreasing parameters the warm flow compaction method can produce complex-shaped components with low cost.

     

/