XU Long-jiao, DONG Chao-fang, XIAO Kui, SHENG Hai, LI Xiao-gang. Kelvin probe study on initial corrosion of carbon steel and weathering steel under atmosphere with Cl-[J]. Chinese Journal of Engineering, 2010, 32(5): 581-588. DOI: 10.13374/j.issn1001-053x.2010.05.004
Citation: XU Long-jiao, DONG Chao-fang, XIAO Kui, SHENG Hai, LI Xiao-gang. Kelvin probe study on initial corrosion of carbon steel and weathering steel under atmosphere with Cl-[J]. Chinese Journal of Engineering, 2010, 32(5): 581-588. DOI: 10.13374/j.issn1001-053x.2010.05.004

Cl-作用下碳钢和耐候钢大气初期腐蚀的Kelvin探针研究

Kelvin probe study on initial corrosion of carbon steel and weathering steel under atmosphere with Cl-

  • 摘要: 利用扫描Kelvin探针(SKP)技术,结合腐蚀产物的形貌分析和物相分析,研究了Q235碳钢和Q450耐候钢在盐雾腐蚀实验早期阶段的腐蚀行为和电位分布.结果表明,Cl-对碳钢有强烈的侵蚀作用,在盐雾腐蚀过程的初期,金属表面出现明显的阴极区和阳极区,表面电位随时间逐步正移,呈现局部腐蚀的特征,且由于合金元素的作用,Q450耐候钢腐蚀较为均匀,SKP测试的表面电位高于Q235碳钢,形成的锈层较为致密,耐大气腐蚀性能优于Q235碳钢.

     

    Abstract: The scanning Kelvin probe (SKP) technique, in combination with energy dispersive spectrum (EDS) analysis of corrosion products, was employed to investigate the initial corrosion behavior and potential distribution of Q235 carbon steel and Q450 weathering steel during salt spray test. The results showed that Q235 carbon steel was severely attacked by Cl-. During the initial period of salt spray test, anodic and cathodic areas formed on the surface of the specimens and the surface potential became more and more positive in the corrosion procedure with a distinct character of localized corrosion. The SKP results showed that Q450 weathering steel was inclined to uniform corrosion, whose surface potential was more positive than that of Q235 carbon steel, probably being due to the effect of alloying elements. The product layer of Q450 was more compact, which indicated that Q450 was more resistive to atmospheric corrosion than Q235.

     

/