杜松林, 金友林, 高振波, 杨应东, 包燕平. VN微合金钢中Ti脱氧夹杂物诱导晶内铁素体析出行为[J]. 工程科学学报, 2010, 32(5): 574-580. DOI: 10.13374/j.issn1001-053x.2010.05.018
引用本文: 杜松林, 金友林, 高振波, 杨应东, 包燕平. VN微合金钢中Ti脱氧夹杂物诱导晶内铁素体析出行为[J]. 工程科学学报, 2010, 32(5): 574-580. DOI: 10.13374/j.issn1001-053x.2010.05.018
DU Song-lin, JIN You-lin, GAO Zhen-bo, YANG Ying-dong, BAO Yan-ping. Precipitation behavior of inclusion-induced intra-granular ferrite in Ti-deoxided VN microalloyed steel[J]. Chinese Journal of Engineering, 2010, 32(5): 574-580. DOI: 10.13374/j.issn1001-053x.2010.05.018
Citation: DU Song-lin, JIN You-lin, GAO Zhen-bo, YANG Ying-dong, BAO Yan-ping. Precipitation behavior of inclusion-induced intra-granular ferrite in Ti-deoxided VN microalloyed steel[J]. Chinese Journal of Engineering, 2010, 32(5): 574-580. DOI: 10.13374/j.issn1001-053x.2010.05.018

VN微合金钢中Ti脱氧夹杂物诱导晶内铁素体析出行为

Precipitation behavior of inclusion-induced intra-granular ferrite in Ti-deoxided VN microalloyed steel

  • 摘要: 通过热力学计算及热态实验,研究了Ti脱氧VN微合金钢中,含Ti夹杂物析出行为及其诱导晶内铁素体析出行为.结果发现,夹杂物与铁素体、珠光体之间的相对位置关系存在六种形式,通过赋予这些形式不同的诱导能力系数,定量比较夹杂物类型、尺寸与诱导能力的关系.Ti的复合氧化物诱导能力最强,Al2O3最弱.Ti的复合氧化物诱导最佳尺寸4~6μm,其他夹杂物最佳尺寸为2~4μm.通过控制夹杂物种类、尺寸促进晶内铁素体析出,能够细化晶粒.

     

    Abstract: Precipitation behaviors of Ti-containing inclusions and inclusion-induced intragranular ferrite were investigated by thermodynamic calculations and laboratory experiments. The results show that there are six forms about position relations of inclusions to ferrite grains and pearlite grains. The effects of inclusion types and size on the inclusion-inducing ability were analyzed quantificationally by defining the index of inducing ability. It is indicated that the ability of Ti-containing complex oxide-inclusions inducing intragranular ferrite is the best, but that of Al2O3 is the worst. The optimal size of Ti-containing complex oxide-inclusions is 4 to 6μm and that of other inclusions is 2 to 4μm. Intra-granular ferrite is induced to precipitate by controlling the inclusion types and size, leading to grain refinement.

     

/