郭芳, 李军, 李维, 刘萍. 反浮选法提高细粒径硅钙质磷矿品位[J]. 工程科学学报, 2010, 32(11): 1388-1392. DOI: 10.13374/j.issn1001-053x.2010.11.003
引用本文: 郭芳, 李军, 李维, 刘萍. 反浮选法提高细粒径硅钙质磷矿品位[J]. 工程科学学报, 2010, 32(11): 1388-1392. DOI: 10.13374/j.issn1001-053x.2010.11.003
GUO Fang, LI Jun, LI Wei, LIU Ping. Improving the grade of a siliceous-calcareous phosphate ore with fine size by reverse flotation method[J]. Chinese Journal of Engineering, 2010, 32(11): 1388-1392. DOI: 10.13374/j.issn1001-053x.2010.11.003
Citation: GUO Fang, LI Jun, LI Wei, LIU Ping. Improving the grade of a siliceous-calcareous phosphate ore with fine size by reverse flotation method[J]. Chinese Journal of Engineering, 2010, 32(11): 1388-1392. DOI: 10.13374/j.issn1001-053x.2010.11.003

反浮选法提高细粒径硅钙质磷矿品位

Improving the grade of a siliceous-calcareous phosphate ore with fine size by reverse flotation method

  • 摘要: 以反浮选法分离细粒径硅钙质磷矿中的石英,获得的P2O5品位和回收率都比正浮选法高,其中P2O5回收率提高了大约40%.在烷基胺盐、醚胺盐和季铵盐三种阳离子捕收剂中,以烷基胺盐捕收剂的反浮选效果最佳,P2O5品位和石英去除率可分别提高到30%和60%以上.酸性介质比碱性介质更有利于提高硅钙质磷矿的品位,在碳酸盐脉石存在的情况下,酸性越强的环境越有利于反浮选分离石英.磷酸比硫酸能更好地调节体系的酸性和抑制磷酸盐矿物,且用量较少.优化的捕收剂用量为0.5~1kg·t-1.三种阳离子捕收剂都在矿石表面发生物理吸附,以烷基胺盐的吸附强度最大,所以其具有较好的浮选性能.

     

    Abstract: Reverse flotation was employed to separate quartz from a phosphate ore with fine particle size which contained siliceous and carbonates gangues.The P2O5 grade and recovery were higher than those by direct flotation,especially the P2O5 recovery increased by about 40%.Compared with ether amine salts and quaternary ammonium salts,alkyl amine salts exhibited better flotation results,the P2O5 grade of concentrates and the quartz removal ratio were higher than 30% and 60%,respectively.Acid reagents were more propitious to improve the grade of the siliceous-calcareous phosphate ore than alkaline reagents.Because of the existence of carbonate minerals,a strong acidity condition was more beneficial to separate quartz by reverse flotation.The application of phosphoric acid as a phosphate depressant and pH modifier gave a better usability in comparison with sulfuric acid,and the dosage of phosphoric acid was less than that of sulfuric acid.The optimum collector dosage was 0.5 to 1kg·t-1.The three cationic collectors adsorbed on ore surfaces in physical adsorption,and the adsorption of alkyl amine salts was the strongest,which is likely to explain their preferable flotation performance.

     

/