IF钢连铸坯表层夹杂物

Inclusions in the surface layer of IF steel slab

  • 摘要: 针对国内某厂以BOF-RH-CC流程生产的IF钢连铸坯,采用氧氮化学分析、光学显微镜分析、扫描电镜分析、能谱分析和金属原位统计分布分析等多种分析方法,综合分析了夹杂物的尺寸、数量、分布以及成分等.结果表明,非稳态浇铸下铸坯二次氧化严重,大型夹杂物增多;铸坯宽度1/4位置表层夹杂物数量高于边部和中部;随着距内弧表面距离的增加,Al系夹杂物平均粒度越来越小,大于10μm的夹杂物比例也越来越小;铸坯表层夹杂物含量和粒度明显高于铸坯内部,其中距内弧6 mm处夹杂物总数最多.

     

    Abstract: The sizes,quantity,distribution,and compositions of inclusions in the surface layer of IF slab produced with the BOFRH-CC process were synthetically studied by means of total oxygen and nitrogen content analysis,optical microscopy,scanning electronic microscopy (SEM),energy dispersive X-ray spectroscopy (EDS),and metal original position analysis (OPA). It is found that reoxidation is serious during the unsteady casting period,and the number of large size inclusions increases obviously; the number of inclusions at the position of 1/4 in slab width is higher than that at the edge and the center of the slab; with the increase of the distance to the inner arc surface,the average size of the inclusions drops and the ratio of the inclusions larger than 10 μm decreases; the number and size of inclusions in the surface layer are obviously larger than those in the inner of the slab,and the amount of inclusions at the position of 6 mm from the inner arc surface is the highest.

     

/