易善杰, 尹海清, 殷小龙, 曲选辉, ZHENG Qingjun. Mo2NiB2基金属陶瓷的制备与性能[J]. 工程科学学报, 2015, 37(4): 488-493. DOI: 10.13374/j.issn2095-9389.2015.04.013
引用本文: 易善杰, 尹海清, 殷小龙, 曲选辉, ZHENG Qingjun. Mo2NiB2基金属陶瓷的制备与性能[J]. 工程科学学报, 2015, 37(4): 488-493. DOI: 10.13374/j.issn2095-9389.2015.04.013
YI Shan-jie, YIN Hai-qing, YIN Xiao-long, QU Xuan-hui, ZHENG Qingjun. Preparation and properties of Mo2NiB2 based cermets[J]. Chinese Journal of Engineering, 2015, 37(4): 488-493. DOI: 10.13374/j.issn2095-9389.2015.04.013
Citation: YI Shan-jie, YIN Hai-qing, YIN Xiao-long, QU Xuan-hui, ZHENG Qingjun. Preparation and properties of Mo2NiB2 based cermets[J]. Chinese Journal of Engineering, 2015, 37(4): 488-493. DOI: 10.13374/j.issn2095-9389.2015.04.013

Mo2NiB2基金属陶瓷的制备与性能

Preparation and properties of Mo2NiB2 based cermets

  • 摘要: 采用单质硼粉、镍粉和钼粉结合反应硼化烧结法制备了Mo2NiB2基金属陶瓷,研究了Mo2NiB2基金属陶瓷在烧结过程中的物相转变和尺寸变化以及烧结温度和保温时间对其力学性能和显微组织的影响.结果发现:随着烧结温度升高,材料物相逐渐由单质相变为二元硼化物相和三元硼化物相,并且材料的尺寸先发生细微收缩,再在硼化反应过程中逐渐增加,最后在液相烧结过程中逐渐减小;随着烧结温度升高,Mo2NiB2基金属陶瓷的抗弯强度和硬度先增加后减小,在1290℃达到最大,分别为1346.5 MPa和83.7 HRA,并且硬质相颗粒逐渐粗化;保温时间对材料性能的影响与烧结温度一致,但在保温30min时抗弯强度最大(1453.3 MPa),保温60 min时硬度最大(83.7 HRA).

     

    Abstract: Mo2NiB2 based cermets were prepared using element powders of boride, nickel and molybdenum. The phase transformation and dimensional change in the sintering stage as well as the effects of sintering temperature and holding time on the mechanical properties and microstructure of Mo2NiB2 based cermets were studied. The results show that with the increasing of sintering temperature, the phase gradually transfers from elemental phase to diboride and then to ternary boride phase, the dimension of the cermets also firstly slightly decreases, then obviously increases in the boronizing sintering process, and finally significantly reduces in the subsequent liquid sintering process. The bending strength and hardness of the cermets firstly increase and then decrease when the sintering temperature rises. The cermets sintered 1290℃ for 60 min show the best mechanical properties with the bending strength of 1346.5 MPa and the hardness of 83.7 HRA. Holding time has a similar effect on the mechanical properties of the cermets. When the holding time is 30 min at 1290℃, the bending strength reaches the maximum of 1453.3 MPa.

     

/