Al2O3对连铸保护渣中氟浸出的影响

Effects of Al2O3 on the leaching of fluorine in mold fluxes

  • 摘要: 为了消除保护渣在使用过程中氟溶解到水中造成的危害,提出了开发高Al2O3含量的保护渣.研究了不同含量的Al2O3对保护渣熔渣水浸液中F-质量浓度和pH值的影响,并利用X射线光电子能谱分析了Al2O3含量对保护渣熔渣结构的影响.当Al2O3的质量分数为4%时,保护渣迁移到水中的F-质量浓度为22.8~35.4 mg·L-1,pH值的变化范围为4.0~9.5;当Al2O3的质量分数由4%增加到34%,F-质量浓度和pH值的变化范围均是先急剧减小后略有增加的趋势.X射线光电子能谱分析显示:增加保护渣中Al2O3的含量时,保护渣中Al2O3通过形成Al—F共价键,抑制了氟的浸出.控制保护渣中Al2O3的质量分数在16%~34%的范围,则实验水样中F-质量浓度在4.0~10.0 mg·L-1的范围,pH值在6.5~7.5的近中性范围,可减弱氟浸出造成的危害.

     

    Abstract: In order to eliminate the hazard effects of the leaching of fluorine in mold fluxes,this paper introduces a mold flux with high Al2O3 content. The effects of Al2O3 content on the concentration of F- ions and the pH value of leaching water were investigated,and the dependence of Al2O3 on the structure of mold fluxes was analyzed by X-ray photoelectron spectroscopy(XPS). When the mass fraction of Al2O3 is 4%,the concentration of F- ions in leaching water is about 22.8 to 35.4 mg·L-1,and the pH range is between 4.0 and 9.5. The F- concentration and the pH range initially reduces and then slightly rises again as the Al2O3 content increases from 4% to 34%. The XPS spectra show that the Al-F bond forms in the mold flux when the Al2O3 content increases. This can restrain the dissolution of fluorine in water. Controlling the content of Al2O3 between 16% and 34%,the F- concentration in leaching water is about 4.0 to 10.0 mg·L-1,and the pH range is between 6.5 and 7.5. This is helpful to reduce the hazard effects of the leaching of fluorine in mold fluxes.

     

/

返回文章
返回