李坚, 华一新, 施哲, 田国才, 徐存英. 铜电解液中硫酸质量浓度和温度对明胶分解的影响[J]. 工程科学学报, 2015, 37(5): 580-587. DOI: 10.13374/j.issn2095-9389.2015.05.007
引用本文: 李坚, 华一新, 施哲, 田国才, 徐存英. 铜电解液中硫酸质量浓度和温度对明胶分解的影响[J]. 工程科学学报, 2015, 37(5): 580-587. DOI: 10.13374/j.issn2095-9389.2015.05.007
LI Jian, HUA Yi-xin, SHI Zhe, TIAN Guo-cai, XU Cun-ying. Influence of sulfuric acid concentration and temperature on gelatin degradation in copper electrolytes[J]. Chinese Journal of Engineering, 2015, 37(5): 580-587. DOI: 10.13374/j.issn2095-9389.2015.05.007
Citation: LI Jian, HUA Yi-xin, SHI Zhe, TIAN Guo-cai, XU Cun-ying. Influence of sulfuric acid concentration and temperature on gelatin degradation in copper electrolytes[J]. Chinese Journal of Engineering, 2015, 37(5): 580-587. DOI: 10.13374/j.issn2095-9389.2015.05.007

铜电解液中硫酸质量浓度和温度对明胶分解的影响

Influence of sulfuric acid concentration and temperature on gelatin degradation in copper electrolytes

  • 摘要: 采用透析的方法将铜电解液中相对分子质量大于3500的明胶进行分离,以二喹啉甲酸(BCA)法测定所得明胶质量浓度,研究了硫酸质量浓度和温度对铜电解液中明胶分解规律的影响.铜电解液中Cu2+基本不影响明胶的稳定性;电解液温度升高和硫酸质量浓度增大,都加剧了明胶的分解.在相同温度下,硫酸质量浓度在150~180 g·L-1范围内每增加15 g·L-1,明胶分解反应速率常数增大约1.2倍;而在相同的硫酸质量浓度下,温度在55~70℃范围内每增加5℃,明胶分解反应速率常数增大约1.5倍.对于铜电解生产,电解液中硫酸质量浓度150~180 g·L-1以及温度60~65℃,可推算出电解液在电解槽中停留3~4 h,明胶的分解率达50%~80%;电解液经过完整的一周循环约需6 h,明胶的分解率可达到70%~90%.

     

    Abstract: Dialysis was utilized to separate gelatin whose relative molecular mass is over 3500 from a simulated copper electrolyte,and the concentration of separated gelatin was determined with a bicinchoninic acid(BCA) method. The impact of H2SO4 concentration and temperature on gelatin degradation was investigated. It was found that Cu2+ hardly affected the stability of gelatin. Increases in electrolyte temperature and H2SO4 concentration exacerbated gelatin degradation. For constant temperature,when the H2SO4 concentration increased by 15 g·L-1 in the range of 150 to 180 g·L-1,the reaction rate constant of gelatin degradation enlarged by 1.2 times. For constant H2SO4 concentration,raising the temperature by 5℃ in the range of 55 to 70℃ increased the reaction rate constant of gelatin degradation by 1.5 times. For copper electrolysis production,when the concentration of H2SO4 in the copper electrolyte was 150 to 180 g·L-1and the temperature was 60 to 65℃,it could be estimated that the residence time of the electrolyte in the electrolytic cell was 3 to 4 h and the gelatin degradation rate in the electrolyte reached to 50% to 80%. A complete cycle of the electrolyte in the copper electrolysis system took about 6 h,and at this moment the gelatin degradation rate in the electrolyte reached to 70% to 90%.

     

/