Liu Qing, Hu Xiaohua, Yang Wangyue, Chen Guoliang. Superplastic Deformation at High Strain Rate and Low Temperature of A Ti-12Co-5Al Allog[J]. Chinese Journal of Engineering, 1993, 15(3): 267-271. DOI: 10.13374/j.issn1001-053x.1993.03.023
Citation: Liu Qing, Hu Xiaohua, Yang Wangyue, Chen Guoliang. Superplastic Deformation at High Strain Rate and Low Temperature of A Ti-12Co-5Al Allog[J]. Chinese Journal of Engineering, 1993, 15(3): 267-271. DOI: 10.13374/j.issn1001-053x.1993.03.023

Superplastic Deformation at High Strain Rate and Low Temperature of A Ti-12Co-5Al Allog

  • A Ti-12Co-5A1 alloy sheet with an ultra fine α-Ti+Ti2Co microstructu was obtained after a proper melting process and thermomechanical treatment. The all under this state exhibits very large superplastic elongation at relatively low temperature ar high strain rates. The elongation more than 1 500% was obtained at a strain rate of 3×10-2s-1 and 700℃. The superplastic deformation induced the size increase and shape chan of Ti2Co intermetallic particles. No cavity was found in the specimen after superplast deformation to 500%.
  • loading

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return