ZHANG Ruizhu, GUO Zhimeng. Influential factors of SHS-densification method for solidifying nuclear waste in SrTiO3 synroc[J]. Chinese Journal of Engineering, 2008, 30(12): 1418-1421. DOI: 10.13374/j.issn1001-053x.2008.12.023
Citation: ZHANG Ruizhu, GUO Zhimeng. Influential factors of SHS-densification method for solidifying nuclear waste in SrTiO3 synroc[J]. Chinese Journal of Engineering, 2008, 30(12): 1418-1421. DOI: 10.13374/j.issn1001-053x.2008.12.023

Influential factors of SHS-densification method for solidifying nuclear waste in SrTiO3 synroc

  • SrTiO3 in which Sr2+ is included was solidified by self-propagation high-temperature synthesis (SHS). Some influential factors on the solid dendification were analyzed by experiment. The optimal process parameters for preparing SrTiO3 and composites were determined as the following:the preform density of 56%; the pre-pressure of 10 MPa, the pressing time of 4 s; the high pressure of 300 MPa, the dwell time of 8 s under high pressure.
  • loading

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return