DU Dong-hai, SHEN Chao, CHEN Kai, YU Lun, ZHANG Le-fu, SHI Xiu-qiang, XU Xue-lian. Stress corrosion cracking of cold worked 316L stainless steel in high temperature and high pressure pure water[J]. Chinese Journal of Engineering, 2015, 37(2): 196-203. DOI: 10.13374/j.issn2095-9389.2015.02.010
Citation: DU Dong-hai, SHEN Chao, CHEN Kai, YU Lun, ZHANG Le-fu, SHI Xiu-qiang, XU Xue-lian. Stress corrosion cracking of cold worked 316L stainless steel in high temperature and high pressure pure water[J]. Chinese Journal of Engineering, 2015, 37(2): 196-203. DOI: 10.13374/j.issn2095-9389.2015.02.010

Stress corrosion cracking of cold worked 316L stainless steel in high temperature and high pressure pure water

  • The stress corrosion cracking growth behavior of 316L stainless steel, which is used as nuclear auxiliary pipelines, was continuously monitored by a direct current potential drop method under a constant stress intensity factor K of 33 MPa·m1/2. By comparing the cracking behavior of this material at 200, 250, 280 and 325℃ in 2 mg·L-1 oxygenated water and deoxygenated water, we found that the crack growth rate is faster in the oxygenated water than in the deoxygenated water. Experimental results also show that there is a peak of the crack growth rate of this material in the deoxygenated water at 250℃, while the crack growth rate increases with the rise of temperature in the oxygenated water.
  • loading

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return